♻️ Concrete Incoming Inspection

Composite compliance check for concrete and masonry: scores compressive strength, impermeability grade and environmental pass rate.

📐 工作原理與說明
逐項按規範限值判定(≤ 上限 / ≥ 下限 / 落在區間內),全部符合判合格,任一不符即不合格
本頁把三項實測值與固定閾值逐項比較,僅供自檢,不生成檢測報告、不作驗收依據;純前端執行,資料不上傳。
GB/T 50081 混凝土≥30 MPa
GB/T 50082 抗滲等級≥P8
GB 6566 放射性達標率≥90%

Formula & Standard References

Item Formula / Note Source / Standard
Concrete compressive testStandard 150 mm cube at 28 d; estimated strength fcu,e corrected ×0.95 for non-standard specimensGB/T 50081-2019 Test Methods for Concrete Physical and Mechanical Properties
Rebound hammer methodRebound values converted to strength with carbonation correction; valid 14–1000 dJGJ/T 23-2011 Technical Specification for Rebound Method Testing
Impermeability gradeP6/P8/P10/P12 withstand 0.6/0.8/1.0/1.2 MPa stepped water pressureGB/T 50082-2009 Long-term and Durability Test Methods of Ordinary Concrete
Environmental acceptancePre-acceptance pollutant testing; Class I buildings formaldehyde ≤0.07 mg/m³GB 50325-2020 Standard for Indoor Environmental Pollution Control

📚 深度解析:混凝土進場三項檢測判定(抗壓/抗滲/環保)

💡 常見使用場景

  • 混凝土材料自檢:按抗壓強度、抗滲等級、環保達標率三項判定
  • 結構安全:抗壓強度是承載力根本
  • 報告可用性:三項全合格方可用於結構驗收
方法
逐項判定:抗壓強度≥30MPa、抗滲等級≥8 級、環保達標率≥90%;三項均滿足為合格。抗壓強度對應設計等級(如 C30),抗滲等級對應抗滲標號(如 P8)。
算例
抗壓 35MPa(≥30 ✓)、抗滲 8 級(≥8 ✓)、環保 94%(≥90 ✓):三項全合格 → 合格。若抗壓降到 25MPa 則不合格,低於 C30 設計、須退場。

❓ 常見問題(FAQ)

抗滲等級和抗壓強度有關係嗎?
二者相關但不等價:高強混凝土通常更緻密、抗滲更好,但仍須分別檢測;抗滲不足會滲漏鏽蝕鋼筋,影響耐久。
三項合格就能澆築?
僅代表材料進場自檢合格;實際澆築還須配合比、坍落度、試塊留置與同條件養護強度,以現場檢測報告為準。
⚠️ 使用說明與注意事項