📋 Wear-Resistance Assessment (Archard)
Evaluate wear resistance with the Archard wear equation.
📐 计算公式
Archard 耐磨链:HRC 查 HRC-HV 表线性插值得 HV(表 20↔226 至 68↔940,越界取端点),H = HV × 9.81(MPa);磨损系数 K = 1×10⁻⁴ × μ²;比磨损率 Ws = K ÷ H;磨损深度率 = Ws × 接触压力 × 滑速(mm/s),×3600 化 mm/h,1000h 深度 = 深度率 × 3.6×10⁶(mm)。校验:任一参数为 0 或非数报「请输入有效的参数」。判据(Ws):<10⁻⁶ A 极低磨损、<10⁻⁵ B 低、<10⁻⁴ C 中等、<10⁻³ D 高、≥10⁻³ E 严重;1000h 深度 ≥1mm 红色警告。
由材料硬度、摩擦系数、接触压力与滑动速度,依据磨损系数与摩擦系数关联的经验简化式综合评估耐磨性。
💡 Archard 方程:比磨损率 Ws = K ÷ H;磨损深度率 wd = Ws × P × v(K 为磨损系数,H 为硬度 MPa,P 为接触压力,v 为滑动速度)
Formula & Standard References
| Item | Formula / Note | Source / Standard |
|---|---|---|
| Wear volume (Archard model) | V = K · ( F · s ) / H, with K the wear coefficient, F the normal load, s the sliding distance and H the hardness | Archard JF (1953), Contact and rubbing of flat surfaces, J. Appl. Phys. 24 |
| Wear rate | Wear rate is the worn volume per unit sliding distance or per unit time | ASTM G99, Standard Test Method for Wear Testing with a Pin-on-Disk Apparatus |
| Role of hardness | In the Archard model, increasing hardness reduces the wear volume | Archard JF (1953), Contact and rubbing of flat surfaces |
| Range of the wear coefficient | K spans many orders of magnitude and must be determined by tests under similar conditions | ASTM G99, Standard Test Method for Wear Testing with a Pin-on-Disk Apparatus |
⚠️ 注意事项
- HRC 硬度自动转换为维氏硬度(HV)再换算为 MPa:H(MPa) = 9.81 × HV
- 磨损系数 K 按经验公式估算:K ≈ 1×10⁻⁴ × μ²(μ 为摩擦系数)
- 实际磨损受润滑条件、表面粗糙度、温度等多种因素影响,结果仅供参考
- 按 Enter 快速计算,Ctrl/Cmd + Enter 复制结果
- 本工具纯前端运行,数据不会上传到服务器
🕘 最近计算
暂无计算记录